Main > WATCH > Ceramics > Zirconia. > Co.: CH. A > Patent > Claims Etc > Claim 1: Sintered Zirconia Article > with Metallic Appearance Comprise > Previously Sintered Article Heated > at > 800C Time=20-180 min.; in



at > 800C Time=20-180 min.; in's subsections
H2-Contg Plasma. Claim 4:

at > 800C Time=20-180 min.; in's products