Product USA. T. No. 1

PATENT ASSIGNEE'S COUNTRY USA
UPDATE 07.99
PATENT ASSIGNEE This data is not available for free
PATENT CLAIMS Process for hydro-treat. charge hydrocarbon feed contg comp. boiling > 1000F & S, metals, for reduction of boiling point & redn of S, metal & C residue content; using as catalyst
- Porous alumina support contg < 2.5% silica on finished cata
lyst basis & bearing 2.2-6% of Group VIII metal oxide, 7-24%
Group VIB metal oxide & < 6% of P oxide
- Said catalyst having Total Surface Area 215-245 square.m
per g, Total Pore Vol. 0.82-0.98 cc/g, Median Pore Diam.
by Surface Area 91-104 angstroem, Pore Diam. Distribution
wherein 22-33% of Total Pore Vol. is present as macropo
res of diam. > 250 angstroem; 67-78% present as micropo
res of diam. +/- 25 angstroem about Pore Mode by vol.
of 86-99 angstroem, 30-35% of Total Pore Vol. present as
micropores with diam. < 100 angstroem & < 0.08 cc/g of
micropore vol. as micropores with diam. < 80 angstroem