OBSERVATION'S See code 8436
TECHNOLOGY Exposing SWNT to NH3 (1%) causes a conductance decrease by 2 orders of magnitude within 2 min.
A drawback so far is the slow recovery of sensor from nanotube-analyte interaction. At room T the nanotubes take hours to release the analyte & be usable again