PATENT CLAIMS Mfg process
- Heat. Zn to > 720C to form molten Zn
- Passing molten Zn through small openings onto a cooling
region formed by a movable surface & maintained at -200C
the Zn forming small particles as it passes through opening
& solidified instantaneously solidified particles as it contac
ts movable surface
- Subjecting solidified particles to grinding process to reduce
solidified particles to size 2-20 square.mm