Main > METALS. > Anodized Metal > Sealing Process

Product DE. H.

PATENT ASSIGNEE'S COUNTRY Germany
UPDATE 08.99
PATENT ASSIGNEE This data is not available for free
PATENT CLAIMS Anodized metal is contacted for 0.5 - 2 min per micrometer of anodized coat. thickness with aq soln at T = 75C - boil. T & pH 5.5 - 8.5 & comprising
- Alkali metal ions (0.0001 - 5 g/l)
- Cyclic polycarboxylic acids (0.0005 - 0.5 g/l) having 3 - 6
-COOH groups
The aq soln contg larger quantity of metal ions than is required for complete neutralization of the acids
PATENT PHOTOCOPY Available on request

Want more information ?
Interested in the hidden information ?
Click here and do your request.


back