PATENT GRANT DATE 16.11.1999
PATENT TITLE Catalyst presulphuration process using two different presulphuration agents

PATENT ABSTRACT The invention concerns a novel presulphuration process for a hydrocarbon conversion catalyst. Presulphuration is preferably carried out offsite (ex-situ). The catalyst presulphuration process is characterized in that a presulphuration agent is used which contains (a) at least one first sulphur compound with a decomposition point T1 of less than 220.degree. C. and (b) at least one second sulphur compound with a decomposition point greater than about 220.degree. C.

PATENT INVENTORS This data is not available for free
PATENT ASSIGNEE This data is not available for free
PATENT FILE DATE June 14, 1994
PATENT FOREIGN APPLICATION PRIORITY DATA This data is not available for free
PATENT CLAIMS We claim:

1. In a process for presulphurizing a hydrocarbon conversion catalyst, the improvement comprising employing a presulphuration agent containing (a) at least one first sulphur compound having a decomposition point T1 of less than 220.degree. C. and (b) at least one second sulphur compound having a decomposition point T2 greater than about 220.degree. C.

2. A process according to claim 1 wherein said first sulphur compound contains at least one --S--S-- or --S--C-- structure.

3. A process according to claim 1 wherein said second sulphur compound has a structure comprising at least one sulphur atom bonded to at least one oxygen atom.

4. A process according to claim 1 wherein said first sulphur compound contains at least one --S--S-- or --S--C-- structure and said second sulphur compound has a structure comprising at least one sulphur atom bonded to at least one oxygen atom.

5. A process according to claim 4, wherein said first sulphur compound is selected from the group consisting of (a) organic polysulphides, (b) elemental sulphur, (c) a combination of sulphur and vegetable oil or a material resulting from a vegetable oil and (d) a combination of sulphur and an olefin, and wherein said second sulphur compound is selected from the group consisting of (a) sulphones, (b) sulphoxides, (c) sulphonic acids, (d) sulphates, (e) sulphites, (f) sulpholanes and derivatives of (c)-(f).

6. A process according to claim 5 wherein the catalyst contains at least one metal selected from the group consisting of molybdenum, nickel, cobalt and tungsten.

7. A process according to claim 1, wherein the first sulphur compound and the second sulphur compound produce amounts of sulphur and the weight ratio between the amount of sulphur produced from the first sulphur compound and that from the second sulphur compound is between 100:1 and 0.5:1.

8. A process according to claim 1 as applied to offsite presulphuration of a catalyst.

9. A process according to claim 1 wherein the second sulphur compound is dimethylsulphone or sulpholane.

10. A process according to claim 1 wherein the catalyst comprises a cobalt-molybdenum, nickel-molybdenum or nickel-tungsten pair.

11. In catalytic hydrodesulphurization or hydrotreatment reactions in a hydrogen atmosphere, the improvement comprising employing as the catalyst a presulphurized catalyst according to claim 1.

12. A process according to claim 7, wherein the weight ratio is between 50:1 and 1:1.

13. A process according to claim 11, wherein hydrotreatment is conducted of crude oil fractions in units not provided with gas recycling apparatus.

14. A process according to claim 1, wherein the catalyst comprises a nickel and tungsten based catalyst.

15. A process according to claim 13, wherein the catalyst comprises a nickel and tungsten based catalyst.

16. A process according to claim 1, wherein the decomposition temperature of the second sulphur compound is greater than 250.degree. C.
PATENT DESCRIPTION BACKGROUND OF THE INVENTION

Presulphuration of hydrocarbon conversion catalysts, primarily for hydrotreatment and hydrodesulphuration and preferably offsite, is carried out in order to fix a sulphur compound on a solid before loading into a catalytic reactor unit. This has been described in our U.S. Pat No. 4,719,195 and European patent EP-A-448 435. During reactor start-up, the sulphur compound decomposes and rapidly and homogeneously sulphurizes the metal oxides present on the catalyst surface to transform them into the sulphide by reaction with the hydrogen present.

The sulphur compound is a polysulphide which is either introduced as a tertiononyl polysulphide by impregnating the catalyst, or a polysulphide is formed on the solid surface by combination of elementary sulphur with an olefinic compound in a vulcanization type reaction (see French patent application 92/04 051).

Reactor start-up generally consists of heating the unit in a hydrogen rich gas. The heating rates are generally between 5 and 50.degree. C./hour.

When the sulphur compound is a polysulphide, sulphur and hydrogen react together in the reactor at temperatures generally between 100 and 200.degree. C., to produce hydrogen sulphide H.sub.2 S which then sulphurizes the oxides in the catalysts. The reactions can be written as follows for a catalyst containing nickel and molybdenum metals:

--S--+H.sub.2 .fwdarw.H.sub.2 S (1)

MoO.sub.3 +H.sub.2 +2H.sub.2 S.fwdarw.MoS.sub.2 +3H.sub.2 O(2)

NiO+H.sub.2 S.fwdarw.NiS+H.sub.2 O (3)

This process operates well and optimally activates the catalysts in the majority of cases. Nevertheless, improvement is necessary in some instances, in particular in two cases which are cited by way of non exhaustive examples. The first concerns catalytic units for the hydrotreatment of crude oil fractions which units are not provided with gas recycling apparatus. In this case, during the activation step in hydrogen with an increasing temperature, a certain amount of H.sub.2 S is formed which is not captured by the metals. This quantity is low, an the order of a few per cent of sulphur with respect to the total weight of sulphur introduced. A first means of limiting this loss is to introduce a slightly higher initial amount of sulphur than stoichiometrically necessary. However, the absence of gas recycling apparatus means that the catalyst is constantly supplied with gas which is free of H.sub.2 S and at high temperature, for example 250.degree. C., 300.degree. C. or 350.degree. C., well above the decomposition temperature of the sulphur compound. The partial pressure of H.sub.2 S in the voids in the catalyst is thus very low. Thus the final stage in the formation of the active phase, namely recrystallization involving atom migration, must be carried out in a non zero partial pressure of H.sub.2 S.

The second instance where conventional techniques are in need of perfecting is where nickel and tungsten-based catalysts are to be activated. Tungsten has a chemistry which is similar to molybdenum, with slight differences: most importantly in this case, the formation kinetics for the active NiS.WS.sub.2 phase are slower than that of the NiS.MoS.sub.2 pair. Thus the final temperature of the activation phase for tungsten is ideally 350.degree. C. to 400.degree. C., whereas for molybdenum based catalysts it is typically between 300.degree. C. and 350.degree. C. At this higher temperature, an absence of H.sub.2 S can seriously and adversely affect phase formation and thus catalyst activity, because of possible formation of WO.sub.2 type species, ie, oxides of quadrivalent tungsten, accompanied by sintering. Nickel and tungsten based catalysts are therefore difficult to activate properly since they are both presulphurized by polysulphide type compounds and the unit is not provided with a gas recycling system.

SUMMARY OF THE INVENTION

The invention relates to the use of other types of sulphur compound whose decomposition temperatures are significantly higher than those of polysulphides in order to generate hydrogen sulphide at temperatures typically of between about 200.degree. C. and 350.degree. C. These novel compounds can be used alone as a sulphurizing agent, but in accordance with the invention they are used with at least one other sulphur compound, preferably mixed with at least one polysulphide. Optimally, a fraction of the sulphur is liberated as hydrogen sulphide at a temperature of about 150.degree. C. and the remainder is produced at about 220.degree. C. (preferably 250.degree. C. to about 300.degree. C.). The partial pressure of H.sub.2 S is thus sufficient across the entire temperature range during the activation period.

The invention thus concerns a presulphuration process, preferably offsite, for a hydrocarbon conversion catalyst, wherein presulphuration of the catalyst is carried out using a mixture containing (a) at least one first sulphur compound with a decomposition point T1 less than about 220.degree. C. and (b) at least one second sulphur compound with a decomposition point T2 greater than about 220.degree. C., preferably greater than 250.degree. C. (decomposition measurements normally determined under hydrogen).

The first sulphur compound generally has a --S--C-- or --S--S-- type structure. Non-limiting examples are organic polysulphides, elemental sulphur, a combination of sulphur and vegetable oil (or a rape seed oil) and sulphur associated with an olefin, ie, the sulphur compounds claimed as sulphurising agents in the patents cited above, namely U.S. Pat. No. 4,719,195, EP-A-448 435 and FR 92/04051.

The second sulphur compound or sulphurizing agent has a structure in which at least one sulphur atom is bonded to at least one oxygen atom. Non-limiting examples are sulphones (alkyl, aryl, alkylaryl and arylalkyl sulphones) or sulphoxides, sulphonic acids and derivatives thereof, sulphates (ammonium, etc . . . ), sulphites (ammonium, etc . . . ), sulpholanes and sulpholane derivatives. Examples of sulphoxides and/or sulphones are dimethyl sulphoxide (CH.sub.3 SOCH.sub.3), diethyl sulphoxide (C.sub.2 H.sub.5 SOC.sub.2 H.sub.5), decyl methyl sulphoxide (CH.sub.3 SOC.sub.10 H.sub.21), dodecyl methyl sulphoxide (CH.sub.3 SOC.sub.12 H.sub.25), dodecyl hydroxyethyl sulphoxide (C.sub.12 H.sub.25 SOC.sub.2 H.sub.4 OH), dimethyl sulphone (CH.sub.3 SO.sub.2 CH.sub.3) and sulpholane (C.sub.4 H.sub.8 SO.sub.2). Examples of sulphonic acids and their derivatives are methyl sulphonyl chloride (CH.sub.3 SO.sub.2 Cl), methane sulphonic acid (CH.sub.3 SO.sub.3 H), methane sulphonamide (CH.sub.3 SO.sub.2 NH.sub.2), ethyl sulphonyl chloride (C.sub.2 H.sub.5 SO.sub.2 Cl) and ethane sulphonic acid.

The weight ratio between the amount of sulphur produced from the first sulphur compound and that from the second sulphur compound is between 100 and 0.5, preferably between 50 and 1.

The invention further concerns the use of catalysts which have been presulphurized using the above techniques, in conversion reactions in particular hydrocarbon hydroconversion reactions and most particularly hydrodesulphurisation and hydrotreatment reactions. These are carried out, for example, in the presence of catalysts based on at least one metal or metal compound selected from the group constituted by molybdenum, chromium, tungsten, cobalt, nickel, and most particularly nickel-molybdenum and nickel-tungsten pairs. The catalyst is used in a hydrogen atmosphere.

PATENT EXAMPLES This data is not available for free
PATENT PHOTOCOPY Availabe on request

Want more information ?
Interested in the hidden information ?
Click here and do your request.


back