PATENT CLAIMS Process for devulcanizing cured rubber into devulcanized
rubber capable of being recompounded & recurred into useful rubber prodts comprising
- Heat. cured to 150 - 300C under pressure > 3.400.000 Pas
cals in the presence of 2-butanol producing a slurry of de
vulcanized rubber in 2-butanol
- Separating devulcanized rubber from 2-butanol