Main > PAPER & PULP > Sheet > Comminution Sheet > Cellulose Fiber Comminution Sheet > Disintegration Energy Redn Method > Debonding Agent Use > Alum. CaCO3. Kaolin. TiO2. ZnO

Product USA. B

PATENT ASSIGNEE'S COUNTRY USA
UPDATE 12.00
PATENT ASSIGNEE This data is not available for free
PATENT CLAIMS Method of reducing the energy required to disintegrate a comminution sheet formed from cellulose fibers without reducing the absorbency strength or fluid transport properties of airfelts formed from comminuted fibers, said method consisting
(a) Forming an aq slurry of cellulose fibers
(b) Adding debonding agent to slurry to coat fibers in fibers wherein debonding agent is selected from group (see title), said agent being added in amount effective to reduce the energy required to disintegrate title sheet formed from coated fibers by 15-50% from amount of energy required to disintegrate sheets formed from uncoated fibers
(c) Forming coated fibers into comminution sheet
PATENT PHOTOCOPY Available on request

Want more information ?
Interested in the hidden information ?
Click here and do your request.