PATENT ASSIGNEE'S COUNTRY | Germany. Japan |
UPDATE | 01.00 |
PATENT ASSIGNEE | This data is not available for free |
PATENT CLAIMS | Cellulose multifilament yarn which is a lyocell multifilament yarn & has a breaking tenacity of 2.8-4.0 g/d (2.5-3.6 g/dtex) & breaking elongation of 13-20% both as dried & which gives a tenacity-elongation curve passing a tenacity range of 0.2-1.0 g/d (0.18-0.90 g/dtex) at an elongation of 5% & a tenacity range of 0.4-2.5 g/d (0.36-2.3 g/dtex) at an elongation of 10% |